17-4 PH stainless steel can be used for a variety of industries including pump shafts, oil path, mechanical seals, and within the aerospace industry. Its composition is carbon, chromium, columbian + tantalum, copper, manganese, nickel, phosphorous, silicon, and sulfur.

Below you will find typical applications of 17-4 PH stainless steel as well as the metals composition and mechanical properties.

Typical usage is seen in applications requiring high strength and a modest level of corrosion resistance. Strength and toughness desired can be manipulated by temperate range in the heat treatment process.

Bar Specification

UNS Type AMS ASTM Characteristics

S17400

17-4 PH

5622
5643

A-564

Combines excellent corrosion resistance, high strength/hardness, low temperature hardening and good fabricating characteristics.

Chemical Composition

Grade C Mn P S Si Cr NI Mo

17-4 PH

0.07

1.0

0.04

0.03

1.0

15. – 17.5

3-5

3-5

Mechanical Properties

Grade Tensile Strength (MPa) mi Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness Rockwell B

17-4 PH

160

145

5.0

35